Corrosion Resistance NBR Material Foamed Rubber Coated Metal RCM
Product Summary
Product Details
Corrosion Resistance NBR Material
,Foamed Rubber Coated Metal RCM
,NBR Material Foamed Rubber Coated
Product Description
MC8020-NBR Foamed Rubber-Coated Metal (RCM) - Oil and Fuel Resistant with High Wear and Corrosion Resistance
The MC8020 is an advanced composite sealing material, engineered through a specialized process that evenly coats a Nitrile Butadiene Rubber (NBR) layer onto a robust metal steel core. This innovative design combines the mechanical strength of steel with the unique elastic properties of NBR, creating a versatile gasket solution for demanding industrial applications.
- Enhanced Conformance to Rough Surfaces: Unlike traditional rubber-coated or soft metal gaskets, the NBR layer on the MC8020 delivers a significantly higher degree of surface conformance. It effectively fills surface irregularities, scratches, and imperfections commonly found on worn or rough sealing flanges, eliminating the need for expensive surface refinishing and ensuring a leak-tight seal even on suboptimal substrates.
- Low Clamp Load Requirement: Thanks to the compliant nature of the NBR coating, the MC6020 achieves an effective seal with substantially lower bolt torque or clamp loads compared to conventional steel or high-density gaskets. This reduces stress on flange bolts, minimizes the risk of flange deformation, and simplifies installation—particularly in lightweight equipment or applications with limited access.
| Property | Specification | |
| Rubber Type | Foamed NBR | |
| Base Metal Type | SPCC | |
| Surface Appearance | Semi-luster black | |
| Overall Thickness (mm) | 0.80±0.20 | |
| Base Matel Thickness(mm) | 0.20±0.01 | |
| Base Metal Hardness (HV) | 115-150 | |
| Rubber Coating Thickness(mm) | 0.30±0.095(per side) | |
| Max . Operation Temp (℃) | ≤150℃ | |
| Rating Adhesion Test ASTM-D3359 | 100% Residual | |
| Pull Off Test (Mpa) ASTM-D4541-09 | ≥1.0 | |
| Compressibility (%) ASTM F-36 | ≥20 | |
| Recovery (%) ASTM F-36 | ≥45 | |
| Creep relaxation rate (%) ASTM F-38 | ≤20 | |
| Unaged Physicals |
Shore A duromete (Points) ASTM D-2240 |
55~65 |
| Tensile Strength Mpa (Min.) ASTM D-412 | ≥8 | |
| Ultimate Elongatoin ( % min) ASTM D-412 |
≥200 | |
| Heat Aged (70 hrs@100℃) |
Change in Durometer hardness (Points) ASTM D-573 |
—15~15 |
| Change in Tensile Strength ( % max. ) ASTM D-573 | —30~30 | |
| Limit elongation change (%) ASTM D-573 | ≥-50 | |
| Compression permanent deformation(%) ASTM D 395,100℃x22h |
≤25 | |
| Volume Change (% max.) Oil IRM 903, ASTM D-471 |
≤20 | |