IATF 16949 FKM Sealing Material Strong Adhesion Strength FKM Coated Metal
Product Summary
Product Details
IATF 16949 FKM Sealing Material
,Strong Adhesion Strength FKM Coated Metal
,FKM Sealing Material Strong Adhesion Strength
Product Description
BF3530 Rubber Coated Metal is manufactured using stainless steel 301 as the metal substrate. Through a specialized production process, a uniform FKM rubber coating is applied to both sides of the substrate, delivering consistent performance and reliable protection.
This material offers excellent heat resistance, long-term durability, and very low compression set. Compared with traditional non-metallic sealing materials, it provides a significantly longer service life. It is typically used in applications requiring higher pressure, higher temperature, and more stringent sealing performance.
- Stainless steel 301 substrate with uniform FKM rubber coating on both sides
- Excellent corrosion resistance and high temperature resistance
- Strong adhesion strength for dependable sealing performance
- Very low compression set and long-term durability
- Extended service life compared with traditional non-metallic sealing materials
| Property | Specification |
|---|---|
| Rubber Type | FKM |
| Base Metal Type | SUS301 |
| Surface Appearance | Semi-luster black |
| Overall Thickness (mm) | 0.35 ± 0.02 |
| Base Metal Thickness (mm) | 0.30 ± 0.01 |
| Rubber Coating Thickness (mm) | 0.025 ± 0.005 (per side) |
| Max. Short-term Operation Temp (℃) | ≤ 250 ℃ |
| Rating Adhesion Test (ASTM-D3359) | 100% residual |
| Pull Off Test (MPa, ASTM-D4541-09) | ≥ 1.4 |
| Base Metal Hardness (HV) | 430 ~ 470 |
| Unaged Physicals — Shore A Durometer (Points, ASTM D-2240) | 75 ~ 85 |
| Unaged Physicals — Tensile Strength (MPa, Min., ASTM D-412) | ≥ 8 |
| Unaged Physicals — Ultimate Elongation (%, Min., ASTM D-412) | ≥ 175 |
| Heat Aged (70 hrs @ 100 ℃) — Change in Durometer Hardness (Points, ASTM D-573) | -15 ~ 15 |
| Heat Aged (70 hrs @ 100 ℃) — Change in Tensile Strength (%, Max., ASTM D-573) | -30 ~ 30 |
| Heat Aged (70 hrs @ 100 ℃) — Volume Change (%, Max., Oil IRM 903, ASTM D-471) | ≤ 20 |
Specifications are provided for reference and may vary within standard manufacturing tolerances.